MEMSnet Home: MEMS-Talk: Electroplating of Ni over Tungsten
Electroplating of Ni over Tungsten
2009-06-06
Andrea Mazzolari
2009-06-07
Shay Kaplan
2009-06-07
Andrea Mazzolari
Electroplating of Ni over Tungsten
Andrea Mazzolari
2009-06-07
Hi Shay,
thanks for the nice suggestion ;)

Which is the tipical thickness which are provided by this tecnique ? Is it
possible to obtain thickness of 50-100 um ?

Andrea

> The best surface and easiest Nickel coatings are done by the shops that
> plate car body parts, head lamps etc. I use them although some of them
> don't
> really know what thickness they get so they need to be 'educated'
> Shay
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
University Wafer
MEMS Technology Review