A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS curing problems when using plastic masters
PDMS curing problems when using plastic masters
2009-07-14
Mikael Evander
2009-07-14
Lupin
2009-07-20
Ulf Mikael Evander
2009-07-20
Yifan Wu
PDMS curing problems when using plastic masters
Mikael Evander
2009-07-14
Hi.

I've just run into a strange problem. I've previously used several different
materials as master for PDMS molding and never ever had any problems. The other
day I tried using a laser ablated polyester film as a master and the PDMS cured
everywhere except where it was in contact with the polyester. Others in the lab
seem to have seen the same problem when using acrylic masters.

I haven't been able to find anything about it and e-mailed dow corning without a
response. Has anyone else seen this and know why it happens? Evaporating
solvents? Materials that aren't compatible with PDMS for some reason?

thanks in advance!

/Mikael
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics