question about ebeam evaportation of metals
Prasanna Srinivasan
2009-07-31
Hi cfshen,

May I know what exactly you mean when you say dense particles? Are you
seeing clustered islands? What pressure, voltage and current values you have
chosen?

Regards,
Prasanna

On Thu, Jul 30, 2009 at 12:39 AM, Chongfei Shen  wrote:

> Dear all,
>
> I'm using ebeam evaporation to deposit Ti and Al. Both films have dense
> particles observed under microscope. The evporation rates are controlled to
> be 4A/s. The wafers were thoroughly cleaned.
>
> What are the reasons that forms the particles? How to solve this problem?
>
> Thank you very much for your suggestions.
>
> cfshen

--
Thanks & Regards,
Prasanna Srinivasan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing