MEMSnet Home: MEMS-Talk: about platinum etching
about platinum etching
2009-08-08
abhaya joshi
2009-08-10
Yoshi.Sakata_Gmail
2009-08-10
Bill Moffat
2009-08-10
walter
2009-08-10
Miyakawa, Natsuki
about platinum etching
Yoshi.Sakata_Gmail
2009-08-10
abhay,

I do not think that you can have the expected pattern by the etching with
HCL (8):HNO3 (1) solution. You should move to the other way to etch. I think
that the lift-off is the alternate solution for you.

Regards,
Yoshi

-----Original Message-----
hi,

i am doing platinum etching (200nm). i am using HCL (8):HNO3 (1) solution at
70C>

i am observing lot of non uniform etching behavior and lot of undercutting.
can any one suggest how to avoid this.

-abhay joshi
university of pune

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering
Nano-Master, Inc.