Post-bake of AZ photoresit
2009-08-11
Y.Tian
2009-08-12
Shao Guocheng
2009-08-12
antwi nimo
Post-bake of AZ photoresit
Y.Tian
2009-08-11
Hi All,

Would anybody comment the post-bake of developed AZ photoresist? I just found
that the structure swells when I tried to post-bake the sample. Because I am
worrying that the AZ will adsorb moisture from the air and the sample was
prepared weeks ago, I just tried to dry it. Through the thickness direction, it
looks the sidewall is curved when the heat travel through it, which was
straight.

Anybody has experience about this?

Thanks a lot!

Regards,
Yingtao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing