thermally curable glue
2009-08-11
Ulli Hansen
2009-08-11
Brian Stahl
2009-08-13
Kuijpers, Peter
2009-08-14
Fei Wang
2009-08-14
Kuijpers, Peter
2009-08-17
Roger Shile
2009-08-18
Kuijpers, Peter
2009-08-18
Roger Shile
thermally curable glue
Kuijpers, Peter
2009-08-14
Hello,

This is rather thick for spincoating, but I maybe you can use a dry film
 In the past we used a dry film from FujiFilm

Best regards,

Peter Kuijpers
MiPlaza Technology Laboratories
Philips Research Europe
High Tech Campus 04
Postbox HTC-4-1
5656 AE Eindhoven
The Netherlands
Tel.: +31 402743667
        +31 612507027
Email: [email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Fei Wang
Sent: Friday 14 August 2009 11:23
To: General MEMS discussion
Subject: Re: [mems-talk] thermally curable glue

Hi all,

I am also trying to find a good way to do wafer bonding with thick
layer like 60um. Is that possible for SU-8 or BCB?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics
MEMStaff Inc.