Source for Low Stress Silicon Nitride
2009-08-17
Roger Shile
2009-08-17
antwi nimo
2009-08-18
Prasanna Srinivasan
2009-08-18
walter
2009-08-18
antwi nimo
2009-08-25
xudehui0108
Source for Low Stress Silicon Nitride
xudehui0108
2009-08-25
If your beam only consists of silicon nitride, I think low stress nitride should
be adopted. LPCVD silicon rich Si3N4 is a commerical choice for low stress
silicon nitride.

If your beam consists of two or more materials, I think the stress gradient of
the beam should be carefully studied to get a straight beam after release.

xudehui0108


 Roger Shile wrote on 2009-08-18  00:32:18:

Can someone suggest a commercial for low stress silicon nitride with low
stress gradient?
Low stress gradient is important as the films will be used to fabricate
free standing beams which must remain straight when released.
Roger Shile
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer