MEMSnet Home: MEMS-Talk: UV-curing glue, UV-LEDs
UV-curing glue, UV-LEDs
2009-10-04
Christian Engel
2009-10-05
Shay Kaplan
2009-10-05
Prasanna Srinivasan
2009-10-05
Christian Engel
2009-10-09
Becker, Matthias
UV-curing glue, UV-LEDs
Becker, Matthias
2009-10-09
Dear Christian,

The adhesive OP29 you are using cures by UV-light and visible light. The
wavelenght of your UV source must match with the needed wavelength of your
adhesive. For this system you can also use a conventional spotlight. You also
have to check if your glass-type transmits enough (UV) light (filter
characteristic).

If you have to pre-adjust your system there is no need to cure the adhesive
complete. You can also use your UV-adhesive, there is no need for an additional
glue. Pre-cure your system, at the edges, so there is no movement. Then post-
cure your system beyond your bonder.

Otherwise look for some fast curing UV-adhesives such as products from DELO.

Best regards Matthias

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.