A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: wet etch of 2um Si3N4
wet etch of 2um Si3N4
2009-10-30
Nor Hafizah Ngajikin
2009-10-30
Kuijpers, Peter
2009-10-30
Shivalik Bakshi
2009-10-31
Edward Sebesta
2009-10-31
xudehui0108
wet etch of 2um Si3N4
Nor Hafizah Ngajikin
2009-10-30
Dear all,

I've tried to etch 2 micron thickness of Si3N4 using hot H3PO4. The
concentration of H3PO4 is 85w%. I heat the H3PO4 at 150 degree celcius for 1
hour. Unfortunately, this experiment didn't work as expected. None of the
nitride is etch away.

Can anybody share with me your experience on nitride etch using H3PO4.

Thank you.

Hafizah

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review