We've tried to make masks using the same procedure last year. We didn't get
acceptable results mostly because the photoreducing machine that we were using
was too old. Another limiting factor here is the type of the glass mask that
you're using. The results of our experiments showed that it is possible to
acheive resolutions around 5 micron.

Please let us know if you had any progress in this regard.

Behrouz Nikpour


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics