jianqiang gu
2009-11-03
Dave Lewis
2009-11-03
DongJuan Xi
2009-11-03
jianqiang gu
Dicing Polyimide Layer
DongJuan Xi
2009-11-03
use laser at 355 nm wavelength.

On Tue, Nov 3, 2009 at 7:43 AM, Dave Lewis  wrote:
> With features that small, you may be better off laser cutting the parts.
> Dicing through the silicon tends to affect the optical characteristics
> of the part especially areas closer to the saw.
>
> Regards,
> Dave Lewis
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group