Exposing thick resist with stepper
2009-11-04
Figura Daniel
2009-11-04
Robert Black
Exposing thick resist with stepper
Figura Daniel
2009-11-04
Hello MEMS talk,

Does anybody know what will happen if I try to expose relatively thick
positive resist (10 um) with i-line stepper with NA 0.6 and achieve CD
of 10 um? By calculation depth of focus of such projection system is +/-
0.5 um - far bellow thickness I am dealing with. Will it be possible to
resolve? What kind of profile I should expect? Any concerns of using
stepper for such unintended application?

Thank you in advance

Daniel
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing