A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photolithography on a rough surface
Photolithography on a rough surface
2009-11-10
ameya g
2009-11-10
Y.Tian
2009-11-10
Oakes Garrett
2009-11-12
ameya g
2009-11-12
Loren St. Clair
2009-11-12
Dean Hopkins
2009-11-13
ameya g
Photolithography on a rough surface
ameya g
2009-11-12
Thanks for the suggestions. I think spray coating seems to be a very good
solution to my problem. I am from Arizona State University and I am not sure

if I can find a spray coater at my university. If there is anyone on the
mailing
list from ASU who has a spray coater, kindly send me an email.

Thanks,
-Ameya - [email protected]



On Tue, Nov 10, 2009 at 1:50 PM, Oakes Garrett  wrote:

> Ameya,
>
> Spray coating a thin, conformal film of photoresist might be the first
> step to solving your problem.  Using this technique, one can eliminate
> the problems encountered when spinning resist across topography.
> Percent (non-)uniformity can also be decreased to roughly 10%.
>
> Please feel free to contact me directly if you have any further
> questions.
>
> Best Regards,
>
> Garrett Oakes
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.