MEMSnet Home: MEMS-Talk: Stripping SU-8
Stripping SU-8
2010-02-01
Paul Nguyen
2010-02-01
David Pierce
2010-02-01
mikas remeika
2010-02-02
Maria Matschuk
2010-02-02
Robert Black
2010-02-02
Paul Nguyen
Stripping SU-8
Robert Black
2010-02-02
Has any one used KMPR resist from MicoChem?  It is supposed to be similar to
SU-8, but easier to strip.

Robert