patterning sub-micron holes in chromium
2010-02-08
Marc Reinig
2010-02-09
Wendell McCulley
2010-02-09
Daniel Figura
2010-02-09
[email protected]
patterning sub-micron holes in chromium
Marc Reinig
2010-02-08
I would like to place one to several sub-micron holes in a film of chromium
on a glass slide.  The chromium does not have to be very thick, only enough
to block visible light, a few microns thick I think.

Anyone have a recommendation on methods or any services that can provide
this?

Thanks in advance,



Marco

________________________________________________________________

Marc Reinig                           Phone: (831) 459-4362
Laboratory for Adaptive Optics        Fax:   (831) 459-2298
UCO/Lick                              Email: [email protected]
University of California, Santa Cruz
1156 High Street
Santa Cruz, CA 95064
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering