MEMSnet Home: MEMS-Talk: DRIE Grass Cleaning
DRIE Grass Cleaning
2010-02-19
Li. Zhang
2010-02-20
renil kumar
2010-02-20
Li. Zhang
2010-02-22
renil kumar
2010-02-22
Fei Wang
2010-02-22
Li. Zhang
2010-02-23
Li. Zhang
2010-02-23
renil kumar
DRIE Grass Cleaning
renil kumar
2010-02-20
Hi Li. Zhang

       How thick your Al and what depth you etched down to the silicon also
needs hints on the recipe

--- On Sat, 20/2/10, Li. Zhang  wrote:

From: Li. Zhang 
Subject: [mems-talk] DRIE Grass Cleaning
To: "[email protected]" 
Date: Saturday, 20 February, 2010, 3:45 AM

Hi everyone,

After I did DRIE etching on silicon samples, I observed grass existing
in trenches.

I use Al as hard mask. Is there any way I can get
grasses away from these samples?

Thanks,

Li. Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review