dear all,

We are using your Microchem's product - PMMA, the Positive EB resist. But during
our microfabrication process, the tempature is not allowed to be higher than
100°C. But the prebaking tempature of PMMA is always 180°C, or ranging from
140°C to 200°C in the data sheet.

The second problem of PMMA is it can not bear severe RIE(reactive ion ething).

Do you have some suggestion about some resist which property is similar to PMMA
but can be prebaked at lower tempature, 120°C at most, and of course not higher
than 100°C is better. At the same time, it also can have a better performance
when RIEed.

Thank you !

limengyue

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer