Dear all,

I have a small question regarding mixing up of the PDMS base and the hardner
in 10: 1 ratio. Generally it is specified as mixing up of the two in 10:1
ratio by weight. But can anyone tell me whether their will be a lot of
difference in the PDMS property if one use the ratio of 10:1 by volume ( eg.
10ml : 1ml ). Normally we can correlate the weight ratio to volume ratio,
but in that case can anyone please tell me the density of the base and
the hardner ? The density of the PDMS is about 0.97 kg/m3 .

Thanks in advance.

Debashis Maji,
JRF - Texas Instruments & IIT Kharagpur collaborative Project,
PhD Scholar - School of Medical Science & Technology,
IIT Kharagpur, India - 721302
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics
Addison Engineering