A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Au lift off
Au lift off
2010-03-11
li shifeng
2010-03-11
Lin Yu
2010-03-11
Brad Cantos
2010-03-11
Ruiz, Marcos Daniel (SENCOE)
2010-03-11
Prasanna Srinivasan
2010-03-12
mikas remeika
2010-03-12
Wilson, Thomas
Au lift off
Ruiz, Marcos Daniel (SENCOE)
2010-03-11
What exactly is the failure mode you are experiencing?

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of li shifeng
Sent: Wednesday, March 10, 2010 4:44 PM
To: [email protected]
Subject: [mems-talk] Au lift off

Hi, All,

I pattened 100nm lines on the glass substrate. The height of the line is
around 250nm. I used an e-beam evaportor to deposit 5nm Ti and 80nm Au.
I found it is very hard to lift off. What are the possible reasons?  Any
suggestions to succeed with an Au lift off process for smaller patterns?

Thanks!

Shifeng
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing