MEMSnet Home: MEMS-Talk: Does ultrasonic damage metal film during lift-off?
Does ultrasonic damage metal film during lift-off?
2010-03-16
Li. Zhang
2010-03-16
Harsh Sundani
2010-03-17
mikas remeika
2010-03-17
Bill Moffat
2010-03-18
Enrique San Andrés Serrano
2010-03-25
Li. Zhang
Does ultrasonic damage metal film during lift-off?
Harsh Sundani
2010-03-16
Hi Li,

I have successfully lifted-off metal films of similar thickness by a 20-30 min
ultrasonic dip. I don't think it will damage the film.

Regards,

Harsh Sundani
Graduate Research Assistant, University of Toledo, Toledo, Ohio.


> Date: Mon, 15 Mar 2010 23:20:29 -0400
> From: [email protected]
> To: [email protected]
> Subject: [mems-talk] Does ultrasonic damage metal film during lift-off?
>
> Hi all,
>
> I'm doing lift-off using ultrasonic bath after soak my samples in NMP
> overnight. However, some parts are difficult to be lifted off.
> Thus, I increased the ultrasonic cleaning duration. But I'm afraid a long
> ultrasonic cleaning (20-30min) might damage the metal film which is 150nm
> sputtered Al.
>
> Would that be a problem?
>
> Thanks,
>
> Li. Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics