Selective etch of AlGaAs relative to GaAs
2010-03-19
Andrew Irvine
2010-03-20
[email protected]
Selective etch of AlGaAs relative to GaAs
Andrew Irvine
2010-03-19
Hi guys.

I want to do a wet etch which removes AlGaAs (x=0.5) but stops on GaAs
(I guess 10x selectivity would be about the minimum).  The layer is 50nm
thick, beneath a 5nm GaAs cap which I'd remove immediately beforehand
with a non-selective etch.

One etch which did it well in the past is concentrated HF, but we can't
use any kind of HF any more for a couple of reasons, one obvious and one
too dull to go into.

Conc HCl?  Seems, according to some very sparse literature, to do the
job for x>0.7, but it's failing miserably on my x=0.5 so far.

And thoughts?

Thanks!

Andy
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
The Branford Group