MEMSnet Home: MEMS-Talk: ProteK B3 coating layer removal
ProteK B3 coating layer removal
2010-04-02
Xiaoyong Liu
2010-04-06
Kuijpers, Peter
2010-04-03
Paul Nguyen
2010-04-04
Xiaoyong Liu
2010-04-06
Matthew Koch
ProteK B3 coating layer removal
Xiaoyong Liu
2010-04-02
Hi,
    I am using a so-called Protek B3 layer (spin coated) from Brewer Sciences as
a protecting layer for my wafer frontside during KOH wet etching. It serves its
purpose pretty well, but it is very hard to remove. I tried the remover (Protek
remover 100) they suggested as well as acetone overnight.

There is still an apparent layer there after overnight soaking in above
solutions. I also tried to use O2 plasma (as well as CF4/O2 combination), but
with no apparent effect.  I am wondering if someone has any experience with it,
and would share their insight with me. By the way, my sample is on Si substrate
coated with a thin layer of SiN. The features are just metal.

Thanks

Xiaoyong

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing