Dear All,

I have to pattern gold onto PDMS for electrodes fabrication. My device
requirements are such that I can not perform a lift-off. I have tried
etching gold (KI+I2+water) at room temperature. After etching, the
PDMS substrates take a reddish hue. These substrates do not bond to
any other material nor a subsequent layer of PDMS onto it gets cured.
Can anyone please suggest some alternative etchant or some method by
which I can cure subsequent PDMS (have already tried curing it at high
temperature for longer durations). Is there some well defined
chemistry between PDMS and gold etchant which I am missing here?

Thanks
Nidhi
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing