MEMSnet Home: MEMS-Talk: oozing issue at Plating
oozing issue at Plating
2010-05-01
Paul Nguyen
oozing issue at Plating
Paul Nguyen
2010-05-01
 Hi All:

Don't know if anyone has experienced of oozing issue at Plating.  I'm having
this issue at around wafer edge and trying to eliminate it.  Any input or
hint for resolving this issue is appreciated.

Regards,
Paul Nguyen