MEMSnet Home: MEMS-Talk: pyrex/pyrex anodic bonding
pyrex/pyrex anodic bonding
2010-05-18
A.ALLOUCH
2010-05-18
Bill Moffat
2010-05-18
Joseph Grogan
2010-05-19
Starlight
2010-06-02
A.ALLOUCH
2010-06-02
Starlight
pyrex/pyrex anodic bonding
A.ALLOUCH
2010-06-02
Hi,

Thank you for your answer. What about the thikness of SI3N4?

best,

Alaa


Starlight a écrit :
> Hi,
>
> Use an ion barrier such as Si3N4 to trap the Na+ ions, then a glass to
> Si3N4 interface at 400 C should bond.
>
> Best regards,
>
> Julian.

--
Alaa el dine ALLOUCH
Doctorant au LAAS-CNRS-Groupe N2IS
7 Av colonel Roche, 31077 Toulouse
Tél : 05 61 33 78 71

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
The Branford Group
Process Variations in Microsystems Manufacturing