A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Power consumption of piezoelectric transducers
Power consumption of piezoelectric transducers
1998-11-16
Cheol-Hyun Han
Power consumption of piezoelectric transducers
Cheol-Hyun Han
1998-11-16
Hi, everybody:
Does anyone knows or has experience to measure or calculate the power
consumption of ZnO piezoelectric transducers?

Now, I'm trying to measure it and compare with commercial
electromagnetic dynamic acoustic transducers. But,
strangely, piezo acoustic transducers give more power consumption as follows.
But normally, considering the advantage of piezoelectric acoustic
transducers, shouldn't the power consumption of piezoelectric transducer
bellow than the one that of dynamic transducers?

Is there any misunderstanding in my way to measuring the power
consumption ?


Dc resistance = infinity
AC current = 0.36 mA
AC voltage = 7.1Vrms
Therefore, R= 7.1/0.00036 = 1.97E4 ohm
Therefore, P= square(7.1V)/(1.97E4 ohm) = 2.5 mWatt


Dc resistance = 28 ohm
AC current = 4.4 mA
AC voltage = 0.035Vrms
Therefore, R= 8.03 ohm
Therefore, P = square(0.035V)/(8.03 ohm) = 0.15 mWatt


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review