MEMSnet Home: MEMS-Talk: About electrostatic actuation of Si membrane
About electrostatic actuation of Si membrane
2010-06-28
[email protected]
2010-06-28
Albert Henning
2010-06-29
antwi nimo
2010-06-29
Marc Reinig
2010-06-28
Robert MacDonald
2010-06-28
Ning Wu
2010-06-28
Gareth Jenkins
2010-06-29
yasser sabry
2010-06-29
Felix Lu
2010-06-29
Gareth Jenkins
About electrostatic actuation of Si membrane
Marc Reinig
2010-06-29
How thick is your membrane?  What is the size of your actuators?  How are
you measuring deformation?  Could you see a 100nm deformation?

Marco
________________________________________________________________
Marc Reinig                           Phone: (831) 459-4362
Laboratory for Adaptive Optics        Fax:   (831) 459-2298
UCO/Lick                              Email: [email protected]
University of California, Santa Cruz
1156 High Street
Santa Cruz, CA 95064

> -----Original Message-----
> From: [email protected] [mailto:mems-
> [email protected]] On Behalf Of
> [email protected]
> Sent: Sunday, June 27, 2010 8:08 PM
> To: [email protected]
> Subject: [mems-talk] About electrostatic actuation of Si membrane
>
> Hi all,
>     I'm working on a membrane mirror research, the mirror was
> fabricated by anodic bonding of Pyrex 7740 glass to Si wafer.  My idea
> is, by applying voltage between the Al electrodes patterned on glasss
> wafer and the Silicon membrane , the membrane will deform through the
> air gap under the electrostatic force. But, terriblly, obviously no
> deformation was observed when even a 300 V voltage is applied and the
> air gap is only 20 microns. I have tested the whole structure and I'm
> sure that there is no short circuit between the membrane and the Al
> electrode, now, I'm desperate and I hope anyone can save me.
>
>  Joe
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation