Yun-Ching Chang
2010-07-13
Xiaohui Lin
2010-07-13
Yun-Ching Chang
2010-07-14
Peng Peng
Problems pouring PDMS into nano holes
Peng Peng
2010-07-14
Yun-Ching,

Have you tried other type of PDMS. For example, here is a paper from
Whitesides group titled "Improved Pattern Transfer in Soft Lithography Using
Composite Stamps". In this paper, they used hPDMS for very small pattern
transfer. It is probably of your interest.

Peng Peng
Graduate Research Assistant
Department of Mechanical Engineering
University of Minnesota
111 Church Street S.E.,
Minneapolis, MN 55455
Tel: (612) 626-2010
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics