Adhesion promotion layer for Cu electroplating
Ying-Tao Tian
2010-08-16
Hi Joe,

100nm thick Ti will do the job.

Yingtao

________________________________________
From: [email protected] [mems-talk-
[email protected]] On Behalf Of [email protected]
[[email protected]]
Sent: 16 August 2010 13:26
To: [email protected]
Subject: [mems-talk] Adhesion promotion layer for Cu electroplating

Hi everyone,

       I'm working on Cu electroplating to fabricate Cu pad. The 200nm Cu seed
layer is directly sputtered on the silicon dioxide without using adhesion layer.
After about 4 um Cu is electroplated, the Cu is not adhered to the substrate
well, and can peel off very easily. My question is, what kind of material can be
used as the adhesion promotion layer. We have Al, Ti, Ag and Ni in our lab, and
will these metals can act as the adhesion promotion layer? If not, what kind of
material can be used and can be readily removed after the electroplating.
Thanks.

Joe
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering