Grimm, Dr. Daniel
2010-09-05
lamine nait
Safe RIE substrate holder + Al2O3 by ALD etching
lamine nait
2010-09-05
Dear Daniel;

For the safe material I think it is best for your substrate holder and for the
silicon etch process to use ceramic materials like alcatel deep silicon etcher.

For the best recipe of aluminum Al2o3 etching is to use chlorine gaze specially
:  BCl3 with high power.

regards

naitbouda abdelyaminea
naitbouda@cdta,dz
Process Engineer in the Dry etch area
of the Clean Room of the CDTA
Centre de Developpement des Technologies Avancées
Cite du 20 Aout 1956 Baba Hassen,Alger,Algerie

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
The Branford Group
Addison Engineering