Hi Everyone,

I am working on forming thin film thermoelectrets with a system
typically used for anodic or thermal compression bonding, think Suss or
EVG bonder.  I am not having any serious success according to the
electrostatic volt meter.  I have done a good amount of reading but I
figure I am missing something basic.

My main materials are PI-2611 and AF Teflon.   These materials are spin
cast on a Silicon wafer and solvent is baked out at 90C before loading
between "dummy" wafers.

I welcome comments and advice.

Best Regards

Mark Crain
Cleanroom Manager & PhD Student
University of Louisville
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing