vacuum grease used in RIE system
Ivan Baturin
2010-09-26
Hello, Jack!

I have seen the recommendations to use a small drop of turbomolecular  vacuum
pump oil for fixing the samples to table and additionally provide better thermal
contact.
TMP pump oil has low vapor pressure and should not give any significant
deterioration of vacuum.

Regards,
Ivan S. Baturin

> -----Original Message-----
> From: Jack Ma [mailto:[email protected]]
> Sent: Wednesday, September 22, 2010 2:29 AM
> To: [email protected]
> Subject: [mems-talk] vacuum grease used in RIE system
>
> Dear all:
>
>   Can anyone provide a name of vacuum grease which can be used in RIE
> system
> (such as Technics mircro-pd series 800II) to prevent the up side down of
> samples.
> --
> BR.
> Jack,HKU


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review