AMMT KOH etch wafer holder
Kuijpers, Peter
2010-10-04
Hello,

Removal can be done in a O2 plasma (recipe: 60min 1000W 130°C)

Best regards,

Peter Kuijpers
MiPlaza Technology Laboratories
Philips Research Europe
High Tech Campus 04
Postbox HTC-4-1
5656 AE Eindhoven
The Netherlands
Tel.: +31 402743667
         +31 612507027
Email: [email protected]


-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Bhargav Nabar
Sent: Friday 1 October 2010 18:33
To: [email protected]
Subject: Re: [mems-talk] AMMT KOH etch wafer holder

Thank you for your suggestion Mr Kuijpers. Could you please comment on ease
of removal of the parylene layer. What solvent do you use and does
it require any agitation (slow rotating or ultrasonic?). Also how was you
experience with the silicet clamp?

Thank you once again.
Bhargav Nabar
UT Arlington Nanofab
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review