PDMS molding using a PDMS mold
2010-10-11
Shao Guocheng
2010-10-11
馮 嘉襄
2010-10-15
eowin rohan
2010-10-11
Kevin Nichols
2010-10-11
Shao Guocheng
2010-10-14
Liang Zhao
2010-10-15
Guocheng Shao
PDMS molding using a PDMS mold
馮 嘉襄
2010-10-11
Gold coating?


----- 原始信件 ----
寄件者: Shao Guocheng 
收件者: [email protected]
寄件日期: 2010/10/11 (一) 10:42:36 AM
主 旨: [mems-talk] PDMS molding using a PDMS mold

Dear all,

    I have a structure that can only be fabricated with SU-8 in a positive
manner (that is, my SU-8 structure is the same as my final structure, instead of

being a negative as in most SU-8 mold fabrication). But I do need to have this
structure in PDMS. So my plan is to do regular PDMS molding using the SU-8
structure and get a negative PDMS mold. With the negative mold and a second PDMS

molding process, I should have a PDMS structure same as the original SU-8 one.
Has anyone done something like this before? How did you overcome the PDMS to
PDMS sticking problem? I am thinking about surface silanization on the PDMS
negative mold, however is concerning about how well the silanization can be done

on PDMS surface and how long it can last. So if anyone has previous experience
with similar procedure, please give some advice about if this is doable or not
(I do have high aspect ratio structure, 10um wide, 100um tall). Or, is there any

other material that I use to make a negative mold from SU-8 master so the
following PDMS mold maybe easy on that material?

Any input is greatly appreciated and thx in advance.

Guocheng Shao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing