A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: removal of HMDS without affecting the photoresist
removal of HMDS without affecting the photoresist
2010-10-20
Mikael Evander
2010-10-21
Jesse D Fowler
2010-10-21
Gareth Jenkins
2010-10-21
David Casale
2010-10-22
Mikael Evander
2010-10-21
Shay Kaplan
2010-10-21
Bill Flounders
2010-10-26
Bill Moffat
removal of HMDS without affecting the photoresist
Gareth Jenkins
2010-10-21
Could you not simply skip the HMDS? If I recall correctly, I used to coat
resist on glass without it. We would bake it at 300 deg C to thoroughly
dehydtate it first.

Additionally, some standard resists include their own primer.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group