SU8 two layer lithography
Abhishek Jain
2010-10-26
Hi Gareth

I intend to use a different mask for the 15um layer. Do you mean I
should spin, pre-bake, expose, PEB as per spec for the 1st 30um  layer
and then spin, pre-bake, expose, PEB 15um 2nd layer as per spec before
developing the 45um thick 2 layers?

thanks a lot

-AJ

On Tue, Oct 26, 2010 at 3:21 PM, Gareth Jenkins  wrote:
> This is possible. Just process each layer using the softbake and PEB
> parameters for the appropriate thickness single layers (i.e. 30 micron then
> 15 micron). Expose the second layer taking into account the increased
> thickness and develop in one final step.
>
> One thing. I'm not sure of is what effect the different solvent system used
> between the 2000 & 3000 series. It may be safer to stick to the same series.
>
>  On 26 Oct 2010 19:47, "Abhishek Jain"  wrote:
>> Hi
>>
>> I am wondering if someone in this community has prepared SU8
>> lithography wafers in 2 layers.
>>
>> I am attempting to make a 30um high layer of patterns (SU8-2025) over
>> which I want to make another 15um (SU8-3010) high features.
>>
>> In particular, it will be most helpfull to know what adjustments I
>> should make in baking temps, time and exposure dose, times on both
>> layers, if there is any need for that.
>>
>> Thank you very much
>>
>> Abhishek Jain

--
Abhishek Jain
Steele Lab for Tumor Biology
Harvard Medical School
Massachusetts General Hospital
149 13th Street
Charlestown MA 02129

PhD Candidate
Biomedical Engineering
Boston University
44 Cummington Street
Boston, MA 02114

Phone: 617-726-4089(work)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing