MEMSnet Home: MEMS-Talk: copper plating
copper plating
2010-10-26
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-28
Fei Wang
2010-10-28
Mingke Xiong
2010-10-27
Kuijpers, Peter
2010-10-27
Mingke Xiong
copper plating
Mingke Xiong
2010-10-27
Hi, dear Nabhiraj,

Thank you for the advise. The current density needs to be reduced so that we can
have a more uniform layer across the board.

Regards,

Mingke Xiong
AEM, Inc.
6670 Cobra Way
San Diego, CA 92121, USA
858-481-0210 ext. 1660
www.aem-usa.com

________________________________________
From: [email protected] [mems-talk-bounces+mxiong
[email protected]] On Behalf Of Nabhiraj Yalagoud
[[email protected]]
Sent: Tuesday, October 26, 2010 9:10 PM
To: General MEMS discussion
Subject: Re: [mems-talk] copper plating

hello,

current density comes from Cu ions moving from Cu electrode, so keeping
current density same and coating slowly is contradictory. I guess you may
have to make the solution acidic where the current flow will be more and
make lighter solution of Copper sulphate. But what happens to Si layer with
acidic solution we have to think... I guess it is not possible.

    You reduce the current density !  What is the reason?  Why don't you want to
reduce the current density?

Dilute solution is the best alternative for this.

Nabhiraj
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing