Hi,

I'm not able to understand why you are doing two layer if it is
possible to get 45 um thickness of using single layer of coating of
either SU8-2000 series or SU8-3000 series?  If you have to do it
two coat, then use single series to get the desired thickness in two coat
instead of using two different series since solvent driven out of the two
layer system will be problematic.

Good luck!
Parshant
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing