MEMSnet Home: MEMS-Talk: Chrome and Oxide
Chrome and Oxide
2010-11-06
Salam Gabran
2010-11-06
Andrea Mazzolari
2010-11-16
abhaya joshi
2010-11-16
Bhupesh Bishnoi
Chrome and Oxide
Andrea Mazzolari
2010-11-06
> Is there a way to etch chrome oxide ? i tried gold etchant as
> recommended by a memsnet user, but that didn't work.

What do you mean with "gold etchant" ?
I do not know which gold etchant you are using, i use a gold etchant from
sigma aldrich, i do not remember the chemical composition, but it has a
dark red color. Such gold etchant does not etch Cr at all...

Best regards,
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing