MEMSnet Home: MEMS-Talk: Au contact for polysilicon
Au contact for polysilicon
2010-11-15
Elina Iervolino - EWI
Au contact for polysilicon
Elina Iervolino - EWI
2010-11-15
Hello,

We would like to use Ni/Cr/Au metallization to be used for ohmic contact to
polysilicon. Does anyone knows if this stack of layers provides good adhesion to
the polysilicon and prevent diffusion of the Au in the poly?

Any other suggestions?

thanks a lot


Elina Iervolino

PhD student
Delft University of Technology
Office Phone: +31 (0)15-2578040
Web page:www.xensor.nl
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
Nano-Master, Inc.