Dibyadeep Paul
2010-11-15
Pradeep Dixit
2010-11-15
Andrea Mazzolari
2010-11-15
Daniel Figura
lithography on a wafer surface containing deep trenches
Andrea Mazzolari
2010-11-15
Hi Pradeep,

I too am interested in dry-laminated photoresist based lithography.

Could you give me suggestions on where to find such photoresist ?

Thanks and best regards,

Andrea

> You should try Dry-laminated photoresist based lithography.
>
> It is working fine for wafers having etched cavities, as resist does not
> go
> inside the cavities. Some of my wafers have 1-2 mm wide cavities. still i
> can get satisfactory lith results.
>
> Thanks,
> Pradeep
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics