MEMSnet Home: MEMS-Talk: AZ5214E and anodic bonding
AZ5214E and anodic bonding
2010-11-17
Xin Yan
2010-11-18
Grimm, Dr. Daniel
2010-11-18
Bill Moffat
2010-11-19
Andrew Sarangan
2010-11-19
Xin Yan
AZ5214E and anodic bonding
Xin Yan
2010-11-19
Thanks for your advice.

i will have a try.

BR

Xin Yan



On Thu, Nov 18, 2010 at 5:33 PM, Grimm, Dr. Daniel
wrote:

> Hi Yan Xin,
>
> normally I have not very good results using AZ5214 in HF etching processes
> due to adhesion problems. After some time (~1/2 min), HF tends to lift the
> resist (depending on your surface preparation). Furthermore, AZ5214 is not
> resistant against penetration of HF through the resist - you'll get partly
> exposed surfaces after a couple of minutes.
> We use ARP-3510, or even better, ARP-3100 (both from Allresist) for long HF
> etching processes.
>
> I think you burn your resist at 400°C and you might not be able to remove
> it afterwards.
>
> Best
> Daniel

--
Yan Xin
-Pen-Tung Sah MEMS Research Center,
-Xiamen University, CHINA
XMU HOME:
http://memsc.xmu.edu.cn/mems_renchaiduiwu/XuYuan_Chen-Group/index_1.html
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics