Glue for ion beam etching
Grimm, Dr. Daniel
2010-11-23
Hi,

we have an Argon ion beam etcher from Roth & Rau. In this etching
machine, the samples are upside-down. In order to prevent them from
falling into our turbo, we are using silver glue. However, for obvious
reasons (a lot of contamination), I want to change the glue.

Does anyone have experience with a high vacuum glue which is thermal as
well as electrical conductive and which is easy to remove with normal
solvents (acetone, NMP, DMSO, KwikStrip)?

Best wishes
Daniel
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review