MEMSnet Home: MEMS-Talk: WC deposition
WC deposition
2011-01-12
Kuijpers, Peter
2011-01-13
jeff besterman
2011-01-15
Ned Flanders
2011-01-15
Nabhiraj Yalagoud
WC deposition
jeff besterman
2011-01-13
Hi Peter,

Do you mean tungsten carbide?

Jeff Besterman
Addison Engineering
150 Nortech Parkway
San Jose, CA 95134
office phone 408-956-5101
office fax 408-956-5111
www.addisonengineering.com

-----Original Message-----
From: Kuijpers, Peter [mailto:[email protected]]
Sent: Wednesday, January 12, 2011 1:41 AM
To: General MEMS discussion
Subject: [mems-talk] WC deposition

Hi all,

Does anyone of you know a "place" where I can get a layer of
app 5µm  WC. I think it is a CVD process.

Looking forward to any feedback

Peter Kuijpers
Process Engineer
Philips Innovation Services
MiPlaza/TL group
High Tech Campus 04-p5.12
5656 AE Eindhoven
The Netherlands
Phone: +31 402743667
Mobile:+31 612507027, Mobex: +31 402798904
Email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics