A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Thermal Oxide Si Wafers
Thermal Oxide Si Wafers
2011-02-14
Babis
2011-02-14
Edouard Duriau
2011-02-14
Denis Petrov
2011-02-14
Denis Petrov
Thermal Oxide Si Wafers
Denis Petrov
2011-02-14
....you could also try to use Vapour HF techniques if you had equipment
(Primaxx or MEMSSTAR).

Regards,

M.Sc. Denis Petrov
Production engineer

MEMS Foundry Itzehoe GmbH,
Fraunhoferstrasse 1,
25524 Itzehoe
Germany

Phone: +49 (4821) 17 45 54
Fax: +49 (4821) 17 42 50
e-mail: [email protected]


2011/2/14 Babis 

> Hey, All
>
> I have recently purchased Thermal Oxide Si (Highly doped) wafers in order
> to prepare Organic TFT samples. However the wafers are double side deposited
> with SiO2. In order to make contact on the un-polished side, I suppose I
> have to etch SiO2. What methods do you propose for that purpose. Is there
> anything to watch out in order to achieve better results?
>
> Thank you in advance!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering
Tanner EDA by Mentor Graphics