Overcut AZ5214 profile
2011-02-22
Parrish Ralston
2011-02-22
Ad Hall
2011-02-22
Bill Moffat
Overcut AZ5214 profile
Parrish Ralston
2011-02-22
I was wondering if anyone has a recipe for AZ5214 as a negative photoresist
(or any other negative photoresist) that has good step coverage, and overcut
sidewalls.

I have been trying for a while to use positive photoresist as a continuity
layer that resides between a MMIC chip set in a cavity and a Ti/Au seedlayer
for electroplating.  I deposit KMPR on top of the seed layer as an
electroplating mold and the solvents in the KMPR react with the positive
photoresist.  It doesn't seem to matter than I have thickened my seed layer
in attempts to better isolate the two layers.

So I would like to try and use a negative resist which hopefully will hold
up better to the KMPR.  But I still need good step coverage and a good,
overcut sidewalls so my seed layer is still continuous.

Thank you,
Parrish
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering