MEMSnet Home: MEMS-Talk: Conductive paste for UH vacuum
Conductive paste for UH vacuum
2011-04-08
Petru Lunca Popa
2011-04-11
Maria Matschuk
2011-04-11
[email protected]
2011-04-13
Maria Matschuk
Conductive paste for UH vacuum
Maria Matschuk
2011-04-11
We once used art clay silver 650 paste:

http://www.artclayworld.com/cartgenie/prodList.asp?scat=417

but it will harden and turn into pure silver at that temperature.

maria

________________________________________
From: Petru Lunca Popa [[email protected]]
Sent: 08 April 2011 11:13
To: General MEMS discussion
Subject: [mems-talk] Conductive paste for UH vacuum

Hi everyone,

Any idea for a silver or gold paste suitable for use at 10 -8 torr and
at high temperatures (around 800 C) ?

Thank you
Petru
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Nano-Master, Inc.