Fahd,

wet etching is probably the worst way of structuring PMMA. Why would you
want to do it this way? You can mechanically mill, hot emboss, wire imprint,
injection mold, laser ablate or laser cut PMMA and each of these methods is
better than etching it.

Cheers
Holger
--
Dr. Holger Becker
microfluidic ChipShop GmbH
Stockholmer Str. 20
D-07747 Jena
Germany

Geschäftsführerin: Dr. Claudia Gärtner
Sitz der Gesellschaft: D-07745 Jena, Germany
Amtsgericht Jena: HRB 209251
USt.-IdNr.: DE 221812444




-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]] Im
Auftrag von Fahd Ali
Gesendet: Dienstag, 10. Mai 2011 14:15
An: [email protected]
Betreff: [mems-talk] PMMA etching


Hello everyone,

      I am using this service for the first time.

I want to do wet etching of PMMA substrate. Does anyone have any idea how to
do it. I want to make small channels in it.

thanking you in advance.
regards,
Fahd
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group