Electroplating Ni on Cr thin film
2011-05-23
Xiaohui Lin
2011-05-23
Hamood
2011-05-23
[email protected]
2011-05-23
Xiaohui Lin
2011-05-24
Shay
Electroplating Ni on Cr thin film
Xiaohui Lin
2011-05-23
I am trying to electroplate Ni (1um thick) bars on Cr thin film (50nm) which
serves as a seed layer.

But after electroplating, I found the adhesion is very weak. Using tweezers
can easily scratch the Ni bar off the Cr surface without any damage to the
Cr surface, which indicates very weak adhesion.

I know that Cr may oxidized in air. Does the oxidation count for the weak
adhesion?

Did anyone has similar experiences? I am crazy now:P

Thanks ahead.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing