MEMSnet Home: MEMS-Talk: Si3N4 etching using H3PO4
Si3N4 etching using H3PO4
2011-07-27
jumril yunas
2011-07-27
Bill Moffat
2011-07-27
Andrea Mazzolari
2011-07-28
jumril yunas
2011-07-27
Kirt Williams
2011-07-27
[email protected]
2011-07-27
Bill Moffat
Si3N4 etching using H3PO4
[email protected]
2011-07-27
If possible try a hi temp oxidation of the nitride, pattern resist, quick boe
etch then etch the nitride.

-----Original Message-----
Date: Wednesday, July 27, 2011 11:31:27 am
To: "jumril yunas" ,"General MEMS discussion" 
From: "Bill Moffat" 
Subject: Re: [mems-talk] Si3N4 etching using H3PO4

Vacuum vapor prime.  I can do free tests.  Bill Moffat
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Nano-Master, Inc.
Mentor Graphics Corporation